环氧地坪漆表干时间是不是越短越好?
发表时间:2021-02-09     阅读次数:     字体:【

环氧地坪漆表干是指环氧地坪漆材料涂装操作形成湿环氧地坪漆涂膜到检查测定表面干燥的这段时间,通称为表面于燥时间,简称为“表干”,触摸不粘手且不会产生印痕。环氧地坪漆表干检测方法:表干在涂装操作现场做检测,常用最简单的操作方法是“指触法”。

Epoxy floor paint surface drying refers to the period from wetland floor paint coating formed by coating operation to surface drying checked and determined. It is commonly referred to as surface drying time, referred to as "surface drying" for short. It does not stick to hands and does not produce marks. Epoxy floor paint surface dry detection method: surface dry in the painting operation site for testing, commonly used the simplest method of operation is "finger touch method".

地坪漆涂料涂装后妥善放置一定时间,目测湿地坪漆涂膜表面含有的溶剂已挥发涂料流平成膜,这时,用手指背轻轻接触涂膜表面,指背检测地坪漆涂膜干燥程度操作。指触的表面几个点处,当手指离开后,指背皮肤上未沾有涂料,指触处无痕迹,则认为该地坪漆涂膜已表干。

Place the floor paint properly for a certain time after painting. Visually observe that the solvent on the surface of the wetland floor paint has been leveled to form a film. At this time, gently touch the surface of the film with the back of your finger, and test the drying degree of the floor paint film with the back of your finger. When the finger leaves, there is no paint on the skin of the back of the finger, and there is no trace on the finger contact, the floor paint film is considered to be dry.

陕西金盛科新材料科技有限公司是一家集研发、生产、销售、施工及技术支持一体化的高科技企业,公司生产基地位于环境优美的安康经济开发区,占地50余亩,拥有全自动地坪材料生产线,现代化实验室及防静电不发火检测设备。公司自成立以来,始终坚持以人为本、诚信立业的经营原则,荟萃业界精英,拥有多名技术骨干,本科及以上学历骨干15名,具有专业的施工技术人员150多人,并有多人获得一.二级建造工程师及注册安全工程师证书。为了开发出真正适合企业需求的防静电不发火地坪材料,企业与西安交通大学、长安大学、陕西科技大学等建立长期合作。联系电话:18192033063 18292511128 15332676171 地址:陕西省西安市灞桥区矿山路988号东方罗马花园2-1308室

 